Inconel 718 Steel Parts

 

Inconel 718 Chemical composition

Alloy

%

Ni

Cr

Fe

Mo

Nb

Co

C

Mn

Si

S

Cu

Al

Ti

718

Min.

50

17

balance

2.8

4.75

           

0.2

0.7

Max.

55

21

3.3

5.5

1

0.08

0.35

0.35

0.01

0.3

0.8

1.15

 

 
Inconel 718 Physical properties

Density

8.2 g/cm³

Melting point

1260-1340 ℃

 

 
Inconel 718 Alloy minimum mechanical properties in the roomtemperature

Alloy

Tensile strength Rm N/mm²

Yield strength R P0. 2N/mm²

Elongation A 5 %

Brinell hardness
HB

Solution treatment

965

550

30

≤363

 
718 Characteristic as below:
 1. workability
2. High tensile strength,endurance strength,creep strength and rupture strength at 700℃.
3. High inoxidability at1000℃. 4.Steady mechanical performance in the low temperature.
5. Good welding performance.
 
 
Inconel 718 Metallurgical structure
718alloy is Austenitic structure, precipitation hardening generate “γ” made it excellent mechanical performance. G rain boundary generate “δ” made it the best plasticity in the heat treatment.
 
Inconel 718 Corrosion resistance
718 alloy with extremely resistance to stress corrosion cracking and pitting ability in high temperature or low temperature environments, especially the inoxidability in the high temperature.
 
Inconel 718 Application field:
The elevated temperature strength, excellent corrosion resistance and workability at 700℃ properties made it use in a wide range of high requirement environments.
 
1.Steam turbine
2.Liquid-fuel rocket
3.Cryogenic engineering
4.Acid environment
5.Nuclear engineering
 
 